4/6 35 minutes
Mix resin, wet out the starboard stringer with glass along with 2nd side of both bulkheads with 1708 on all 3.
Tonight i will sand and flush router all of the edges. gut glass for the pop side of the stringers. laminate the port stringer. Glass the starboard side stringer 2nd side.
SO far i have used 1.5 gallons of epoxy 50/50 resin with some loss as expected on the edge seepage. I would estimate a loss of about 1.5 cups which is not bad. But i will tell you that 1708 drinks the resin. But it is thick structural glass so that is to be expected.
I am still on track to glass the stringers and bulkheads into the hull this week as planned. If i can stay on schedule i will be a happy camper.
It was 8* cooler last night in the shop and it is apparent that that drop is at the viscosity threshold of the chemical state of the resin. this batch was a bit more yellow milky color and a tad thicker than my last work way. 64* int he shop vs 72*. food for thought. this morning the set up was finger print minimal tack as i had expected being a little cooler last night.
Weather forecast for the next 10 days is 73-88* with a low of 54 one night. so this is nice. I hope that the 40% rain on sunday does not happen. as i may have to glass in on sat AM. Also hope the sunday rain does not happen as i planned to go to the inwatter boat show at the marina. BUT the temps are good for glass70s-80 are great in my book. fast enough cure times but not 100* where a batch could kick too fast and waist half a tub before applied. Which i freaking hate.


_________________
Not Penny's Boat
1993 190 Horizon 5.0L EFI http://www.smwebhead.com/phpBB3/viewtopic.php?f=3&t=111361977 14' CMF Skiff SOLD
2015 Emotion Stealth Angler 11